You are on page 1of 1

Yogunluk Akışkanlık Fırınlanma Sıcaklığı (Drying Fırınlanma Süresi

Firma Kodu Hammadde Cinsi


(Density) (Melt Flow Rate) Temperature) (Drying Time)
Basell EP548R Polyproplen 0,9 g/cm3 21 g/10 min Yok Yok
3
Basf 165H Polystyren 1,045 g/cm 3,5 g/10min Yok Yok
3
Basf Escrimo Polystyren 1,029 g/cm 3,6 g/10min Yok Yok
Borealis BE170MO Polyproplen 0,902 g/cm3 13 g/10 min Yok Yok
Styrene Butadiene
Edistir SR200 1,04 g/cm3 14 g/10 min Yok Yok

Edistir RC600 Polystyren 1,04 g/cm3 6 g/10 min Yok Yok


Edistir ICE R835D Polystyren 1,04 g/cm3 3 g/10 min Yok Yok
3 0
Magnum 8391 ABS 1,05 g/cm 28 g/10 min 80 C 3-4 Saat
Cycoloy
Sabic HC1204HF PC+ABS 1,15 g/cm3 24 g/10 min 100-110 0C 2-4 Saat

Cycoloy
Sabic PC+ABS 1,18 g/cm3 22 g/10 min 100-110 2-4 Saat
FXC810SK
Sabic 815F PBT+PET 1,43 g/cm3 16 g/10 min 120 2-6 Saat
Styron 485 Polystyren 1,05 g/cm3 12 g/10 min Yok Yok
3
Styron 634 Polystyren 1,05 g/cm 3,5 g/10 min Yok Yok
3
Styron 637 Polystyren 1,05 g/cm 2,5 g/10 min Yok Yok